Norm

ISO 8076:1984

Issue date: 1984 10 01

Aerospace process — Anodic treatment of aluminium alloys — Chromic acid process 40 V DC, undyed coating

Gives requirements for producing and testing. Sealed anodic coatings are applied to improve resistance to corrosion and as a pretreatment for painting. Unsealed anodic co...
Read more
Withdrawn : 2005 05 02
Publisher:
International Organization for Standardization
Format:
Digital | 3 Pages
Language:
English

Gives requirements for producing and testing. Sealed anodic coatings are applied to improve resistance to corrosion and as a pretreatment for painting. Unsealed anodic coatings provide a suitable surface for the application of structural adhesives and allow increased durability for paints. Gives information on technical requirements, quality assurance provisions, packaging and delivery.